Low Creep Material Designed For Forehearth Roof Blocks

As changes in forehearth design have required forehearth roof blocks to be made in more complex shapes, creep behaviour has become a vitally important part of the material selection process. It has also driven the development of a material specifically designed for forehearth and distributor roof blocks.

Author
Un-named
Origin
Unknown
Journal Title
Glass Industry 82 3 March 2001 16-17
Sector
Refractories
Class
R 390

Request article (free for British Glass members)