Love Beer - Hate Oxygen (Barrier Packaging For Plastic Bottles)

Plastic bottles are widely used for soft drinks as an alternative to glass; however, their use for beer requires anoxygen-barrier layer. High-performance resins and barrier layers can prevent oxygen from entering PET containers and retain carbon dioxide. There are an estimated 17 different barrier formulations, some of which are discussed in this article. SurShield from Owens-Illinois uses SurShot multilayer injection technology to supply the exact amount of barrier material for each wall. Constar's product, Oxbar, provides up to 110 days of shelf life for beer, and more than a year for citrus juices. Other companies manufacturing barrier containers include Amcor PET Packaging and Evalca. Voridian, a division of Eastman Chemical, has a Web page (the Oxygen Limited Shelf Life Calculator) that enables customers to model shelf life for new PET containers. Information is given on two tests for assessing barrier effectiveness.

Author
H Behar
Origin
Unknown
Journal Title
Beverage World 122 2 Feb 2003 42-45
Sector
Container glass
Class
C 4533

Request article (free for British Glass members)

Love Beer - Hate Oxygen (Barrier Packaging For Plastic Bottles)
Beverage World 122 2 Feb 2003 42-45
C 4533
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.