Long-Range Granular Feature Of Silicate Glasses And Its Relation To Glass Properties

Numerous experimental results show that silica and silicate glasses consist of higher density granules about 20 to 50nm sized and lower density linkages. Such long-range feature should originate from the long-range density fluctuation of the glass-forming liquid. Due to the highly co-ordinated network structure of glass, the lower density regions may be under strain. Following this assumption many phenomena of glass observed here and reported in the literature can be explained well, e.g. anomalous conductivity, brittleness, granular boundary contour of crack, high conductivity on the fracture surface, cloudy damage after dishwashing, corrosion products on glass surface, distribution pattern of Ag colloidal particles in float glass bath side, disproportional large influence of water on glass properties, etc.

Author
C Wang
Origin
University Bayreuth, Germany
Journal Title
Glass Sci Technol 78 6 2005 279-286
Sector
Special Glass
Class
S 3042

Request article (free for British Glass members)

Long-Range Granular Feature Of Silicate Glasses And Its Relation To Glass Properties
Glass Sci Technol 78 6 2005 279-286
S 3042
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.