Logopak Pulls Off Quinn Glass Deal

Quinn Glass chose Logopak from a list of 13 manufacturers to supply over 35 pallet labelling units for its new UK plant. At Quinn's factory at Elton, near Chester, Bottles are sent to either to a high bay warehouse with 280,000 pallet locations; directly to the customer; or, to the onsite filling hall for filling, labelling and shipping.

Author
Un-named
Origin
Unknown
Journal Title
Packaging Magazine Feb 9 2006 1
Sector
Container glass
Class
C 3050

Request article (free for British Glass members)