Local Structure Of Alkaline-Earth Boroaluminate Crystals And Glasses: Ii, 11B And 27Al Mas Nmr Spectroscopy Of Alkaline-Earth Boroaluminate Glasses

Magic angle spinning nuclear magnetic resonance spectra of alkaine-earth boroaluminate glasses have shown that the structures of these glasses are far more complicated than previously thought. Analysis of the data provides a qualitative model that can be used to predict compositional variations.

Author
B C Bunker Et Al
Origin
Sandia National Laboratories, Univ Of Illinois, Spectral Data Services
Journal Title
J Am Ceram Soc 1991 74 6 1430-1438
Sector
Special Glass
Class
S 558

Request article (free for British Glass members)

Local Structure Of Alkaline-Earth Boroaluminate Crystals And Glasses: Ii, 11B And 27Al Mas Nmr Spectroscopy Of Alkaline-Earth Boroaluminate Glasses
J Am Ceram Soc 1991 74 6 1430-1438
S 558