Liquidus Temperatures In Silicate Glasses

Thermodynamic calculation of liquidus temperatures in multicomponent systems has advanced far enough to justify a comparison with results calculated using equations based on regression analysis on large sets of experimental determinations. The first attempts to find empirical models were don by the mid 1970s. These models were, however, restricted to rather narrow composition ranges or to given primary phase fields. A model covering a fairly large set of compositions was developed within a joint venture between Philips, Saint-Gobain and the universities of Sheffield and Abo Akademi. Their model was based on fifty glasses in the system Na20-K20-Mg0-Ca0-Sr0-Ba0-Pb0-Al203-B203-Si02. This paper extends the set of data used and compares liquidus temperature estimates obtained by the models with temperatures obtained by thermodynamic calculation.

Author
K H Karlsson Et Al
Origin
Abo Akademi University, Finland
Journal Title
Icg 2 Extended Abstracts 2001 78-79
Sector
Special Glass
Class
S 2588

Request article (free for British Glass members)

Liquidus Temperatures In Silicate Glasses
Icg 2 Extended Abstracts 2001 78-79
S 2588
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.