Liquidus Temperature Of Sro-Al2O3-Sio2 Glass-Forming Compositions

Despite the important role of strontium aluminosilicate glasses in various technologies, there is no available phase diagram for this ternary system in the ACerS-NIST Phase Equilibria Diagrams Database. Establishing the liquidus surface (liquidus temperature T-liq and primary devitrification phase) is crucial for glass composition design, because the liquidus temperature is intricately connected with the glass-forming ability of the melt. In this work, the authors have determined the liquidus surface by X-ray diffraction phase analyses of isothermally reacted samples from powder mixtures of 24 compositions.

Author
B M Abel Et Al
Origin
Corning Inc, New York
Journal Title
Int J Appl Glass Sci 4 3 2013 225-230
Sector
Special Glass
Class
S 4040

Request article (free for British Glass members)

Liquidus Temperature Of Sro-Al2O3-Sio2 Glass-Forming Compositions
Int J Appl Glass Sci 4 3 2013 225-230
S 4040
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
13 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.