Liquidus Temperatues Of Bioactive Glasses

Melts in the composition range of bioactive glasses have their liquidus temperatures within or close to working range. Additionally, bioactive glasses show a strong tenancy to crystallisation due to their composition. Thus many bioactive glass compositions are unsuitable for demanding working procedures such as fibre drawing. In this work we discuss the suitability of different methods for measuring liquidus temperature of bioactive glasses. Thermal analysis was used, and complemented by sintering curves as given by hot stage microscopy. Hot stage microscopy could be used to measure liquidus also when the thermal effect associated with liquidus was low and consequently the DTA was not suitable. Liquids of some glasses was measured with optical microscopy for samples heat treated in a gradient furnace.

Author
H. Arstila Et Al
Origin
Process Chemisrty Centre, Biskopsgatan, Finland.
Journal Title
Advanced Materials Research Vols 39-40 (2008) 287-292
Sector
Special Glass
Class
S 3412

Request article (free for British Glass members)

Liquidus Temperatues Of Bioactive Glasses
Advanced Materials Research Vols 39-40 (2008) 287-292
S 3412
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.