Lining Up The Bottles

Dura Temp has developed the Roller Bottle Guide to solve the problem of misaligned bottles during ware handling at the hot end. The device ensures bottles are lined up correctly on the production line without causing any drag. Instead of using fixed contact material that causes drag, this device employs several freely rotating rollers mounted in an aluminium channel. The rollers present 360 deg/contact surface and last longer than traditional strip-style bottle guides. They are replaceable.