On-Line Viscosity Measurement

A new on-line system for measuring viscosity changes in the glass melt has been introduced. The system analyses the dependency between the physical behaviour of molten glass and a harmonic vibration of a ceramic rod, which is partly immersed in the melt. Practical tests under industrial conditions have led to remarkable results.

Author
Th Richter & A Strack
Origin
Silitec Ingenieurgesellschaft, Silicattechnik Gmbh
Journal Title
Int Glass Review 2/99 50-51
Sector
General
Class
G 2035

Request article (free for British Glass members)