On-Line Oxygen Sensor For The Tin Bath In Float Glass Production Lines

A special oxygen sensor has been developed for the continuous measurement of the equilibrium oxygen pressure and oxygen content in the molten tin in the float bath of the float glass production line. The measuring principle and sensor design are explained. Float glass surface detects like tin pick-up, bloom, scum and tin drops are directly or indirectly caused by too high oxygen levels in the molten tin. Measurements by means of the on-line oxygen sensor are presented. These examples illustrate the merit of such sensor to limit or even prevent defects by a better control of the bath atmosphere.

Author
P R Laimbock & R Beerkens
Origin
Read-Ox Consultancy & Tno, Netherlands
Journal Title
Cesp 27 1 2006 19-32
Sector
Flat glass
Class
F 2240

Request article (free for British Glass members)

On-Line Oxygen Sensor For The Tin Bath In Float Glass Production Lines
Cesp 27 1 2006 19-32
F 2240
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.