Lightweighting Improvements

Much time and resources have been dedicated to developing forming processes and coatings that allow the container manufacturer to produce lighter, more environmentally-friendly packaging to suit today's market requirements. However, little has been said of the glass quality improvements that are necessary to make lightweighting a success. This article explains how supplemental electric heating can help with glass lightweighting.