Lightweighting Improved With Hot End Inspection

Producing containers with less weight puts high demands on the forming process. In order to be successful in lightweighting products, hot end inspection should be added to traditional cold end inspection. In this article the authors, from hot end technology supplier Xpar Vision, explain why they believe this to be true.

Author
Un-named
Origin
Unknown
Journal Title
Glass International Sept/08 31-32