Lightweighting In The Glass Container Industry

Production of lightweight containers by the NNPB process is described.

Author
H Griffel
Origin
Heye-Glass
Journal Title
Ceramic Engng Sci Proc 1987 8 3-4 156-170
Sector
Container glass
Class
C 24