Thomas Edison constructed his first incandescent lamp in 1880 with a glass bulb made from handblown lead glass tubing. Within one short month of this development, Edison realised that bulb making was not one of the strengths of his research facility. This article gives a brief rundown of the evolution of the light bulb, starting with Corning Glass Works agreeing to supply Edison's Menlo Park laboratory with blown glass blanks at $5/gross to today's modern lighting devices.

Author
R C Marlor
Origin
Osram Sylvania Inc, Usa
Journal Title
The Glass Researcher 10Th Anniversary Collection 1986/96 47-48
Sector
Special Glass
Class
S 2581

Request article (free for British Glass members)

Lighting - Glass Technology Updates Industry
The Glass Researcher 10Th Anniversary Collection 1986/96 47-48
S 2581
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
12 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.