Light-Tone Ceramic Facing Brick Manufacture Using Ferrous-Metallurgy By-Products

The principal variational regularities of the properties of ceramic samples obtained from compositions based on combinations of loam, semi-fireclays, and metallurgical slag are examined. The phase composition of and structure formation processes in wall ceramic have been investigated using high-precision modern equipment. The composition of ceramic mix making it possible to produce high-quality ceramic facing brick based on clay raw materials and ferrous-metallurgy by-products is presented.

Author
I G Dovzhenko
Origin
South Russia State Tech University
Journal Title
Glass & Ceramics 68 7-8 Nov/2011 247-249
Sector
Glass Ceramics
Class
GC 769

Request article (free for British Glass members)

Light-Tone Ceramic Facing Brick Manufacture Using Ferrous-Metallurgy By-Products
Glass & Ceramics 68 7-8 Nov/2011 247-249
GC 769