Light Switch

Its a laser, but not as we know it. For a start, you need a microscope to see it. Gleaming eerily green, it is a single spherical particle just a few tens of nanometres across. The tiniest laser ever made revives the idea that we can compute with light, according to this article.

Author
J Mullins
Origin
Consultant Editor
Journal Title
New Scientist 23 January 2010 39-41