Li2O-Sio2-Al2O3-Meiio Glass-Ceramic Systems For Tile Glaze Applications

The devitrification processes of three commercial lithium aluminosilicate glass ceramics have been investigated by differential thermal analysis, X-ray diffractometry, scanning electron microscopy and IR spectroscopy to verify the possibility of using glass-ceramic materials as tile coatings.