A Lens To Bend Rays

This article, taken from Business Week, discusses new ray-bending technology from US firm, Lightpath Technologies. The company has developed a new type of lens, called a gradium lens, which could revolutionise optics and imaging.

Author
O Port
Origin
Unknown
Journal Title
Gmpa 5/97 170-171
Sector
Special Glass
Class
S 1262

Request article (free for British Glass members)

A Lens To Bend Rays
Gmpa 5/97 170-171
S 1262