Lehr Profiling Saves Energy

A temperature profiling system has been developed and is designed to help manufacturers to optimise glass annealing and decorating processes to minimise energy use.

Author
D Plester
Origin
Datapaq, Uk
Journal Title
Glass 78 4 May 2001 121-122
Sector
Container glass
Class
C 1740

Request article (free for British Glass members)

Lehr Profiling Saves Energy
Glass 78 4 May 2001 121-122