Lead Oxide Coatings On Sol-Gel-Derived Lead Lanthanum Zirconium Titanate Thin Layers For Enhanced Crystallization Into The Perovskite Structure

An improved method is described for the sol-gel preparation of PLZT thin layers in the perovskite structure. The method uses a PbO cover coat. Details are reported for the sol-gel processing route and heat-treatment conditions.

Author
T Tani And D A Payne
Origin
Beckman Inst. And University Of Illinois Et Al Urbana-Champaign, Usa
Journal Title
J Am Ceram Soc 77 5 1994 1242-1248