Lead Free Crystal

Since 1991 and in view of the need to comply with new environmental regulations, various research works have been looking at a possible alternative to lead crystal. This paper presents a lead-free crystal which has very interesting properties similar to those of lead crystal (brightness, density, mechanical resistance and the working range).