Lead And Cadmium Free Glasses And Frits

In the field of ceramic tableware, lead has traditionally been used in glazes and low melting fluxes (combined with pigments to form colours). Cadmium has largely been used in the form of cadmium sulphoselenide pigments, to generate red, orange and yellow colours. Cadmium can also feature in fluxes for these colours. This paper largely concentrates on glazes, reviewing unleaded formulations researched and giving an indication of the extent to which the UK tableware industry is converting to unleaded glaze formulations. An initiative by Middlesex and Galway Universities, Galway Crystal & Royal Brierley Crystal is reviewed, addressing the question "how safe are the elements we propose to replace lead with?" through a progrmme of factory dust/volatiles monitoring and metal release testing. Finally, the difficulties of finding replacements is discussed.

Author
I Campbell
Origin
Ceram Research, Uk
Journal Title
Glass Technology 39 2 1998 38-41
Sector
Domestic glass
Class
D 339

Request article (free for British Glass members)

Lead And Cadmium Free Glasses And Frits
Glass Technology 39 2 1998 38-41
D 339
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.