Leaching Kinetics Of Tungstic Acid And In Situ Synthesis Of Tungesten Carbide In Silica Gel Matrix

Leaching of tungstic acid is carried out in ammonium hydroxide solution at two different pH (8 and 10.5), at three different temperatures of 40, 50 and 60 deg C. It is observed that initially, the dissolution rate is very fast followed by decrease in rate with time. It also increases with increase of temperature and pH. The mechanism of isothermal leaching kinetics of tungstic acid in ammonium hydroxide is mainly of contracting geometry type. Ammonium tungstate has been used as a precursor to syntheisze nano tungsten carbide in the silica gel matrix by in-situ generation of hydrogen and extremely find carbon. The size of tungsten carbide is found to be in the nm range.

Author
D Chaira Et Al
Origin
Centre For Nano-Science & Technology, India
Journal Title
Trans Indian Ceram Soc 66 4 2007 167-170
Sector
Special Glass
Class
S 3621

Request article (free for British Glass members)

Leaching Kinetics Of Tungstic Acid And In Situ Synthesis Of Tungesten Carbide In Silica Gel Matrix
Trans Indian Ceram Soc 66 4 2007 167-170
S 3621
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.