Latest Refractory Developments In The Steel Industry

Since the shift from open hearth to basic oxygen process, steel making technology has undergone a gradual development driven by the demands for higher productivity and improved quality.

Author
Un-named
Origin
Unknown
Journal Title
Ind Minerals Sept/2002 44-47
Sector
Refractories
Class
R 445