Latest Generation Of Vision Systems Provide Greater Flexibility

Emhart Glass has launched the ProScanner 200 series of vision base and surface sealing inspectors designed to provide more sophisticated inspection and improved operational simplicity.

Author
R Diehr
Origin
Emhart Glass, Usa
Journal Title
Glass Int 23 2 March-April 2000 17-18