Latest Developments In The Design Of Batch Plants

The factors involved in planning a new batch plant are discussed.

Author
B-H Zippe
Origin
Zippe Industrieanlagen Gmbh
Journal Title
Glass Production Technology International 1990 37-40
Sector
General
Class
G 414