Late-Middle Ages Lead Glass Manufacture In The Environs Of Grunenplan Im Hils (German)

X-ray fluorescence analyses of glasses found in the neighbourhood of Grunenplan are reported and the relevance of the finds to lead glasses found elsewhere in Europe is discussed.

Author
K-H Mader
Origin
Deutsche Spezialglas Ag (Desag)
Journal Title
Glastech Ber 1989 62 12 N73-N75
Sector
Domestic glass
Class
D 78

Request article (free for British Glass members)

Late-Middle Ages Lead Glass Manufacture In The Environs Of Grunenplan Im Hils (German)
Glastech Ber 1989 62 12 N73-N75
D 78