Laser Technique To Treat Coatings

This article outlines a laser technique that is especially useful for treating coatings on glass moulds. In 2010, Chpolansky started to treat coatings on cast iron or bronze base metallic surfaces using a laser technique especially useful for glass moulds. The coating areas aimed at were areas in contact with hot glass (1300-1600 deg C) and more particularly (joining zone), the ring and the neck. The aim is to make these coatings on cast iron and bronze, using the laser beam technique to decrease Thermally Affected Zones (TAZ) and promote thermal properties of the part maintained. Coating is performed under three different techniques in existing prior art: Spray Gun is the traditional method, but is known to give random results; The TIG Process uses rods, but is expensive and is not adapted to mould coating; and Plasma Transferred Arc (PTA) technique, currently preferred, in spite of its lack of reproducibility.

Author
M Rege
Origin
Chpolansky, France
Journal Title
Glass International Feb/2014 89
Sector
News Items
Class
N 3208

Request article (free for British Glass members)

Laser Technique To Treat Coatings
Glass International Feb/2014 89
N 3208
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.