Laser Patterning Of Oriented Linbo3 Crystal Particle Arrays In Nio-Doped Lithium Niobium Silicate Glasses

The patterning of LiNbO3 crystals was carried out at the surface of NiO-doped 40Li2O-32Nb2O5-28SiO2 (LNS) glasses using continuous-wave Yb:YVO4 fibre laser (wavelength: 1080 nm) to gain a deeper understanding of the crystal growth in the laser-induced crystallization in glasses.

Author
M Shimada Et Al
Origin
Nagaoka University, Japan
Journal Title
Int J Appl Glass Science 4 9 2018 518-529
Sector
Special Glass
Class
S 4468

Request article (free for British Glass members)

Laser Patterning Of Oriented Linbo3 Crystal Particle Arrays In Nio-Doped Lithium Niobium Silicate Glasses
Int J Appl Glass Science 4 9 2018 518-529
S 4468