Laser-Based Fast And Flexible Surface Structuring Of Glass

Large-area surface structuring of glass is of particular interest for a wide range of applications. Conventional methods such as sandblasting or wet chemical etching technologies have reached their limits in terms of flexibility, process velocity and pollution. With the alternative of a laser-based surface structuring, all disadvantages of the current structuring methods can be avoided.