Landglass has, over the years, introduced many new products to the market, some of which are quite influential, such as bending tempering furnaces for auto sidelites, jumbo-size bending tempering furnaces for architectural glass, double curvature bending tempering furnaces and jet heating furnaces, to name a few. In this article, the company presents its most recent development - combined tempering furnaces - which can, says the company, eliminate quality defects such as optical deformation (waviness), spherical bending of thin glass, hot spots on thick glass, white haze and glass breaking inside the furnace.

Author
Un-named
Origin
Unknown
Journal Title
Glass-Tech International 2/2012 46-48
Sector
Flat glass
Class
F 3273

Request article (free for British Glass members)

Landglass - Ongoing Developments - Combined Forced Convection
Glass-Tech International 2/2012 46-48
F 3273
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
12 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.