Laminated Fire Resistant Glass

The new addition to the CGI International range of fire glasses - Fireswiss Foam - provides, says the UK-based firm, a high quality, fully insulated fire glass, which can be cut from stock and supplied to meet the demanding needs of site programmes. Fireswiss Foam is made by a special laminating process which creates adjacent layers of glass and clear silicate built up to create a complete fire barrier to both the spread of fire and heat. Depending on the overall glass thickness, fire performances of 30 up to 60 minutes and more can be achieved in a wide range of suitable frame types. For more information please see: www.cgii.co.uk

Author
Un-named
Origin
Unknown
Journal Title
Glass-Tech Int 4/2005 80
Sector
Flat glass
Class
F 1851

Request article (free for British Glass members)

Laminated Fire Resistant Glass
Glass-Tech Int 4/2005 80
F 1851
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.