Laminated Architectural Glass - The Solution For Design Flexibility

This article re-examines, in the light of increased experience and knowledge, the inherent characteristics of laminated glazing in current use with particular attention focused on performance.

Author
Dr T L Tan
Origin
Monsanto Singpore Co (Pte) Ltd
Journal Title
Kanch March 1996 52-57