La203-Al2-3-Si02 Glasses For High-Power, Yb3+ -Doped, 980-Nm Fibre Lasers

Single-mode semiconductor pumps have failed to keep pace with the increasing power requirements of Er-doped fibre amplifiers (EDFAs), so there is a need for high-powered 980-nm sources. Yb3+ -doped tapered fibre lasers can provide high-power output by conversion of a low-brightness, high-powered, 920-nm, multimode broad stripe laser diode to a high-brightness, 980-nm, single-mode output. CVD-based fibre fabrication methods are incapable of delivering fibres with an NA>~0.3 or with good efficiency at 980nm so a new method of high-NA fibre fabrication was developed.

Author
M J Dejneka Et Al
Origin
Corning, Usa
Journal Title
J Am Ceram Soc 85 5 2002 1100-1106
Sector
Glass Fibre
Class
GF 322

Request article (free for British Glass members)

La203-Al2-3-Si02 Glasses For High-Power, Yb3+ -Doped, 980-Nm Fibre Lasers
J Am Ceram Soc 85 5 2002 1100-1106
GF 322
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.