Koa Glass - New Product

The Japanese glass packaging company Koa Glass has developed an anti-bacterial glass maned "Biocomposite Glass Microparticles". The product has antibacterial silver ions embedded within the glass particles, and through an elution speed process, the glass reportedly maintains semi-permanent antibacterial properties. (whole item)