Kibing Glass Malaysia

Kibing Group China announced plans for a float line in Malaysia in 2015. The first glass rolled out from the annealing lehr on 25th April 2017. This article provides an overview of the project.

Author
Un-named
Origin
Unknown
Journal Title
Glass Worldwide June-July 2017 52, 54
Sector
News Items
Class
N 3844a

Request article (free for British Glass members)

Kibing Glass Malaysia
Glass Worldwide June-July 2017 52, 54
N 3844a
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.