Judd-Ofelt Parameters, Hypersensitivity, And Emission Characteristics Of Ln3+(Nd3+, Ho3+, And Er3+) Ions Doped In Pb0-Pbf2 Glasses

Optical properties of Ln3+ ions doped in different crystalline and glass host matrices are of current interest a they exhibit lasting transitions which are influenced by the host material. Glasses as doping matrices have many advantages. A close study of the optical spectra of Ln3+ ions over the entire series looking for differences and similarities between the crystalline and glass hosts should be of value. Two aspects, one pertaining to the variation in the Judd-Ofelt parameters as we look at the rare-earth series and the other pertaining to the influence of the host matrices on the hypersensitive transitions, have been investigated in detail in crystalline matrices unlike in glass systems.

Author
P Nachimuthu & R Jagannathan
Origin
University Of Hyderabad, India
Journal Title
J Am Ceram Soc 82 2 1998 387-392
Sector
Special Glass
Class
S 1608

Request article (free for British Glass members)

Judd-Ofelt Parameters, Hypersensitivity, And Emission Characteristics Of Ln3+(Nd3+, Ho3+, And Er3+) Ions Doped In Pb0-Pbf2 Glasses
J Am Ceram Soc 82 2 1998 387-392
S 1608
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
16 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.