Italian Refractories Update

Italy's SIGMA Group is to double production capacity at its Bulgarian refractories plant in early 2016. This follows the recent completion of significant investments at the Italian factory, involving a doubling of the pre-assembly area, a specially built 5000 sq/m storage area and the installation of a vibrocasting unit for special shapes up to 1800kg. The group reports additional business and major contracts in several countries, including the USA, S America, China, France, Poland and Germany, in addition to a steady increase of turnover with existing customers worldwide. The R&D team has created a series of innovations, including two zirconium-based products for the furnace bottom according to cullet percentage and a special mullite grade for regenerator chambers of highly stressed furnace installations.

Author
Un-named
Origin
Unknown
Journal Title
Glass Worldwide Oct/Nov 2015 18
Sector
Refractories
Class
R 844

Request article (free for British Glass members)

Italian Refractories Update
Glass Worldwide Oct/Nov 2015 18
R 844
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.