Isvv Study Reveals Short Life Span For Wine In Pet Bottles

Wine stored in plastic PET bottles starts to oxidise within 6 months, according to a new study that contradicts claims made b leading supermarkets on the shelf-life of the format. The Institute of Vine and Wine Sciences (ISVV) in Bordeaux carried out the year long study, which found that both the flavour and chemical composition of white wine changed within 6 months of being packed in single- or multi-layer PET bottles or bag-in-box. The wine did, however, remain stable in glass bottles, the study claimed. The ISVV results contradict claims from major retailers, including M&S, and Waitrose, over the shelf life of wine packed in PET bottles. The ISVV is planning to continue the testing for a second year.

Author
Un-named
Origin
Unknown
Journal Title
Packaging News June 2010 10
Sector
Container glass
Class
C 4208

Request article (free for British Glass members)

Isvv Study Reveals Short Life Span For Wine In Pet Bottles
Packaging News June 2010 10
C 4208
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.