[Iran] Iran - Production Rising

Iran produced 167,000/tonnes of glass in the first two months of the current Iranian year, which began 21st March. A rise of 3.7% from last year. In this period, production of glassware, sanitary products and chinaware amounted to 70,600 tonnes, 12,700 tonnes and 6,700 tonnes, respectively.