Ir Spectroscopic And X-Ray Phase Analyses Of Alkali-Free Fluorophosphate Glasses And Their Crystallization Products

Seven glass compositions were synthesised in the systems Ba(PO3)2-MgF2 and Ba(PO3)2-2AlF3.3CaF2. Predominant groups in the 1st system are metaphosphatic, pyrophosphatic, monofluorophosphatic, and MgF2 structural units. In the second system metaphosphate, pyrophosphate and fluoroaluminate groups predominate. Crystallisation products identified were a-Ba2P2O7, BaMgP2O7, a-Ca2P2O7, a-CaF2AlF3, etc.

Author
Vd Khaliley Et Al
Origin
Unknown
Journal Title
Fiz. Khim. Stekla 4 1 1978 42-46
Sector
Primary Papers
Class
PP 1238

Request article (free for British Glass members)

Ir Spectroscopic And X-Ray Phase Analyses Of Alkali-Free Fluorophosphate Glasses And Their Crystallization Products
Fiz. Khim. Stekla 4 1 1978 42-46
PP 1238
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
17 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.