Ionic Conductivity In Glass

Advances in developing new fast ion conductors and understanding the mechanisms of ion conductivity, the mixed mobile ion effect and ac relaxation effects are discussed.

Author
M D Ingram
Origin
University Of Aberdeen
Journal Title
Phys Chem Glasses 1987 28 6 215-234