Ionic Character Of Oxygen And Its Local Structure In Silicate Glasses Containing Alumina

The amphoteric property of alumina in silicate glasses has been investigated in terms of the electronic polarisability of oxygen.

Author
T Yagi Et Al
Origin
Tokyo Inst Technology, Japan
Journal Title
Phys Chem Glasses 42 4/5 2001 287-291