Ion Mobility And Structural Relaxation In Glass

A dynamic structural model is described where ions in glass are mobile and are yet part of the glass structure. The model introduces the concepts of memory, mismatch energy, and fluctuating pathways. Condctivity variations in single and mixed-cation glasses have previously been rationalised on this basis. Examined here are some wider implications relative to EXAFS results, internal friction peaks, and the effect which restricted ionic mobility has on the strength/fragility of glass-forming systems.

Author
M D Ingram Et Al
Origin
Univ Of Aberdeen,Scotland
Journal Title
Chimica Chronica, New Series 23 1994 221-226
Sector
Special Glass
Class
S 895

Request article (free for British Glass members)

Ion Mobility And Structural Relaxation In Glass
Chimica Chronica, New Series 23 1994 221-226
S 895
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.