Ion-Exchange Method In Glass Production

An ion-exchange process for use in production of flat glass and items such as filters and gauge glasses has been developed. The thermo-mechanical properties of the chemically-strengthened glasses have been investigated and the effectiveness of their use in various designs and service conditions assessed. Some 12m pieces of chemically-strengthened glass are produced annually in the Soviet Union.

Author
E V Sobolev Et Al
Origin
Unknown
Journal Title
Glass And Ceramics 1989 46 5-6 256-261
Sector
Special Glass
Class
S 5029

Request article (free for British Glass members)

Ion-Exchange Method In Glass Production
Glass And Ceramics 1989 46 5-6 256-261
S 5029