Ion Exchange On Glass Substrates: Influence Of The Mixed Cation Effect On Concentration Profiles

Conductivity measurements have been carried out on silver sodium borate and silicate glasses revealing a "mixed cation effect". This effect is interpreted as being nonlinear variations with glass composition of the self diffusion coefficients of the two mobile cations. An empirical relationship is deduced from conductivity measurements and is introduced into ion exchange governing equations which are solved by numerical method.

Author
C Annequin-Thevenin Et Al
Origin
Lab 'Electrochimie Et Physico-Chimie Des Materiaux, France
Journal Title
Phys Chem Glasses 38 5 1997 263-268
Sector
Special Glass
Class
S 1240

Request article (free for British Glass members)

Ion Exchange On Glass Substrates: Influence Of The Mixed Cation Effect On Concentration Profiles
Phys Chem Glasses 38 5 1997 263-268
S 1240
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
10 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.