Investigation Of Selenium Retention In High Redox Glasses

Laboratory glass melting experiments were made to study the effect of glass redox on selenium retention. Initially, it was found that as expected, selenium retention decreases as glass redox ratio increases. But, unexpectedly, selenium retention then levels off and reaches a minimum upon further increases in glass redox, before once again increasing for very high redox ratios of more than 0.60. Selenium concentrations in the furnace atmosphere at different locations in a commercial float glass furnace were also measured as an indicator of selenium volatility at different stages of glass melting. A study of the effect of glass redox ratio on the spectral absorption of the major selenium containing colouring centres in float glass was also made.

Author
L J Shelestak & M Arbab
Origin
Ppt Ind, Usa
Journal Title
Glass Sci Technol 6 2005 255-260
Sector
Flat glass
Class
F 1945

Request article (free for British Glass members)

Investigation Of Selenium Retention In High Redox Glasses
Glass Sci Technol 6 2005 255-260
F 1945
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.