Investigation Of Properties & Corrosion Behaviour Of Hard Tia1N And Alcrn Pvd Thin Coatings In The 3Wt% Nacl Solution

Physical vapour deposition technique (ion plating, sputtering, and arc evaporation) provides a promising ground for the deposition of hard coatings by the formation of dense adhesive film at low deposition temperatures. In this work, TiAlN and AlCrN coatings were deposited on ASTM-SA213-T-11 steel by using Balzer's rapid coating system (RCS) machine under a reactive nitrogen atmosphere.

Author
V Chawla Et Al
Origin
Iit Roorkee, India
Journal Title
J Aust Ceram Soc 47 1 2011 48-56
Sector
Special Glass
Class
S 3674

Request article (free for British Glass members)

Investigation Of Properties & Corrosion Behaviour Of Hard Tia1N And Alcrn Pvd Thin Coatings In The 3Wt% Nacl Solution
J Aust Ceram Soc 47 1 2011 48-56
S 3674
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 9 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.