An Investigation Of Nanoparticles In Contemporary Lustres On Modern Iznik Tiles

Lustre is defined as "metal-glass nanocomposite thin layer composed by dispersing copper or silver nano particles in silica based glassy matrix." The technique is based on a specific firing of ceramic in a reducing atmosphere in the presence of metallic salts. The result is a surface layer with iridescent reflections of various colours. In the literature, production of lustre in glazed Iznik ceramics has never been reported. In this paper, it is aimed to obtain a lustre layer on tiles fabricated with the formula and procedure copied from the archaeological Iznik tiles.

Author
M Sariguzel Et Al
Origin
Marmara Research Centre, Turkey
Journal Title
J Aust Ceram Soc 51 1 2015 34-39
Sector
Enamels
Class
E 165

Request article (free for British Glass members)

An Investigation Of Nanoparticles In Contemporary Lustres On Modern Iznik Tiles
J Aust Ceram Soc 51 1 2015 34-39
E 165
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
8 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.